http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20110116309-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad0f8fa205a890aa4186a15768fe0e98 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2304-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2301-052 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82B3-00 |
filingDate | 2010-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9e145d434eeffed9b7060391cb06f57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9fa7739b40f3cd5b3ab40090b2c8080 |
publicationDate | 2011-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20110116309-A |
titleOfInvention | Aluminum nano powder and its manufacturing method |
abstract | The aluminum nanopowder according to the present invention is dissolved by heating and stirring AlCl 3 and LiAlH 4 in a molar ratio of 1: 3 in dibutyl ether ((C 4 H 9 ) 2 O), and byproducts are removed by centrifugation. It is formed by heating a 3 AlO (C 4 H 9 ) 2 solution within a set temperature range and then adding TTIP. In addition, the method for producing an aluminum nanopowder according to the present invention is a material preparation step of preparing AlCl 3 and LiAlH 4 , dibutyl ether and thiatiapy as an aluminum precursor, and dibutyl ether as a solvent of the AlCl 3 and LiAlH 4 The by-product input step to dissolve, and by-product generation step of producing a H 3 AlO (C 4 H 9 ) 2 solution and by-products by heating and stirring the dibutyl ether solvent, and by-products generated in the by-product generation step A by-product removal step of removing LiCl, a precursor solution heating step of heating the H 3 AlO (C 4 H 9 ) 2 solution from which the by-product is removed to a set temperature, and the heated H 3 AlO (C 4 H 9 ) 2 A catalyst adding step of adding TTIP to the solution, and a powder for preparing aluminum nanopowder by heating and stirring the H 3 AlO (C 4 H 9 ) 2 solution to which TTIP is added for a predetermined time. Characterized in that the manufacturing step The. |
priorityDate | 2010-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |