Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b0736cb19133fba052305970af8f9767 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2523-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2523-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2521-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C2521-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-584 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-52 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J38-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C5-2512 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J38-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J38-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C6-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J38-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C6-04 |
filingDate |
2009-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e2f780ce80b57e9d0bfbf9c17933265 |
publicationDate |
2011-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20110107332-A |
titleOfInvention |
Catalyst regeneration |
abstract |
The present invention discloses the regeneration of used catalyst mixtures comprising (i) an isomerization catalyst comprising magnesium oxide and (ii) an inorganic carrier and a metathesis catalyst comprising at least one of molybdenum oxide and tungsten oxide. The method comprises the steps of (a) decoking the catalyst mixture used in the presence of an oxygen-containing gas to produce a decked catalyst mixture; (b) contacting the decked catalyst mixture with steam at a temperature in the range of 100 to 300 ° C. to produce a regenerated catalyst mixture. |