abstract |
The present invention has a density of less than 950kg / m 3 obtained by polymerisation with a single site catalyst, 10 to 20g / 10 minutes MFR 21, four or more shear thinning index SHI 2.7 / 210, and preferably at least 60% It relates to a multimodal ethylene polymer having a degree of crosslinking. |