abstract |
In the present invention, low-PAH-containing carbon black (A) 17 to 75 mg / g of iodine (B) a STSA surface area of 17 to 64 m 2 / g, (C) an iodine number of greater than 1.06 mg / m 2: STSA surface area ratio, (D) 60 to 160 ml / 100 g of OAN value, (E) 40 to 110 ml / 100 g of COAN, (F) a mode of greater than 100 nm, and (G) Benzo (a) pyrene content below 2 ppm A rubber mixture comprising at least one rubber and at least one low-PAH-containing carbon black. The rubber mixture can be used to make functional rubber articles and tires. |