http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20100135908-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_87789f5a94acfc089ee0dd3625242d9a |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-2406 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B23-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B23-0461 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B5-10 |
filingDate | 2009-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c87c5e286385c0cdbd8473cee23e31b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7a93845bcb4184e719f0029a580eeeaa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d8a8419a6fde89a086d9ab297284f00 |
publicationDate | 2010-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20100135908-A |
titleOfInvention | Process for producing nickel and cobalt using metal hydroxides, metal oxides and / or metal carbonates |
abstract | The method of producing a metal oxide from a metal salt selected from the group consisting of nickel hydroxide, cobalt hydroxide, mixed nickel-cobalt hydroxide, nickel carbonate, cobalt carbonate and mixed nickel carbonate-cobalt comprises providing a mixture of metal salts, Mixing the metal salt with a binder selected from the group consisting of inorganic binders and organic binders, forming the mixture into aggregates, and calcining the aggregates to produce metal oxides. The metallic nickel or cobalt manufacturing method includes providing a metal salt selected from the group consisting of nickel hydroxide, cobalt hydroxide, mixed nickel-cobalt hydroxide, nickel carbonate, and cobalt carbonate, the metal salt consisting of an inorganic binder and an organic binder. Mixing with at least one binder selected from the group to form a mixture, optionally adding water, forming the mixture into agglomerates, drying the agglomerates, effective reducing amount of coke and / or coal And adding the dried aggregates directly with an effective amount of heat to produce metallic nickel and / or cobalt. Coke particles may be added to the mixture prior to flocculation. The agglomerate may be at least one metal salt selected from the group consisting of nickel hydroxide, cobalt hydroxide, mixed nickel-cobalt hydroxide, nickel carbonate, cobalt carbonate, and mixed nickel carbonate-cobalt; And a binder selected from the group consisting of an inorganic binder and an organic binder. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101367834-B1 |
priorityDate | 2008-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 75.