http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20100124495-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_99f8f8d6219e59bd6f935895edd6b2d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_68b49143b3da6ad513872243730325dc |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61C7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61C7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61C7-20 |
filingDate | 2009-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e322b1f680039758d7716cc9fa927df3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3eba07945d01ca828360705a0738e3e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1316c0d5ffafff198d1c0cdb363ac165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_600146028fefba06337c021a4077df1a |
publicationDate | 2010-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20100124495-A |
titleOfInvention | Corrosion resistance improvement Orthodontic wire manufacturing method |
abstract | The present invention relates to a method for manufacturing an orthodontic wire for improving corrosion resistance, and in the orthodontic wire, a degreasing step for removing impurities from a prepared material surface, an etching step for removing an oxide film of the material from which impurities are removed, and improved adhesion Nickel (Ni) strike step for the surface, surface activation step for activating the nickel-plated material surface, silver strike step for improving adhesion to the activated material surface, silver (Ag) plating step and the silver-plated material It characterized in that it comprises a phosphorus (In) coating the phosphorus (In). The discoloration of the wire of the present invention configured as described above can be minimized, functional requirements can be satisfied, and manufacturing costs can be greatly reduced. |
priorityDate | 2009-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |