abstract |
The present invention comprises the steps of: a) contacting a metal alkoxide with a surface by vapor deposition or immersion deposition; And b) treating the metal alkoxide to conditions suitable for forming an oxide adhesive layer on the surface, wherein the conditions are selected from one or more of the group consisting of pyrolysis, microwave treatment, complete hydrolysis and partial hydrolysis. It relates to a method of activating a surface. |