http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20100024431-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b1784eb7fc902d292db30e120ec712d5 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 |
filingDate | 2008-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1a685e99e8bb4392f865f94137f61c79 |
publicationDate | 2010-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20100024431-A |
titleOfInvention | Spherical copper fine powder and its manufacturing method |
abstract | An average particle diameter of copper fine powder is 0.05 micrometer or more and 0.25 micrometer or less, The spherical copper fine powder characterized by the above-mentioned.n n n Copper slurry is added to an aqueous medium containing an additive of a natural resin, a polysaccharide, or a derivative thereof to prepare a slurry, and a 5-50% acid aqueous solution is added to the slurry at once within 15 minutes to perform a disproportionation reaction. A process for producing spherical copper fine powder by disproportionation reaction.n n n It is an object of the present invention to provide a method for producing copper fine powder which can produce controlled copper particles or particles of metal copper particles, in particular finer copper fine powder quickly, efficiently and stably. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210058910-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180054914-A |
priorityDate | 2007-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 30.