assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-318 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-405 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133519 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1335 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate |
2008-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3da7115ee4662f0b80d3ee5eb7ccb181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4355354d36fe98d4bb08707a522be5b7 |
publicationDate |
2010-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20100013337-A |
titleOfInvention |
Adhesive sheet for optical films, its manufacturing method, adhesive optical film, and image display apparatus |
abstract |
As an adhesive film for optical films which has an adhesive layer on a release sheet, the surface roughness Ra of the adhesive layer surface on a release sheet is 2-150 nm. The said adhesive sheet for optical films is the process of coating an adhesive coating liquid on a release sheet, the said 1st drying process of temperature 30-80 degreeC, a wind speed of 0.5-15 m / sec, and a temperature of 90-160 degreeC to the said adhesive coating liquid. And the manufacturing method which has a process of forming an adhesive layer by performing the 2nd drying process of 0.1-25 m / sec of wind speeds. When the said adhesive sheet for optical films is applied to image display apparatuses, such as a liquid crystal display device, the problem of the visibility associated with an adhesive layer can be reduced. |
priorityDate |
2007-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |