http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20090113300-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D169-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-03 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-02 |
filingDate | 2007-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20090113300-A |
titleOfInvention | Method for producing a solid having a concave shape on the surface |
abstract | As a production method for producing a solid having a concave shape on the surface, which is expected to be applied to various industrial fields at a very low cost and stably, a hydrophilic solvent is used as solvent A and a hydrophobic solvent is used as solvent B. In this case, at least the solvent A, the solvent B, and a solution containing the polymer compound soluble in the solvent B are used to produce a solid having a concave shape on the surface, and the boiling point of the solvent A is the solvent B Is at least a boiling point of and the total mass of the solvent B is 50% by mass or more of the total mass of the solvent contained in the solution, and either or both of the solvents A and B contained in the solution evaporate. The solution is solidified while forming a concave shape by condensation on the surface of the solution. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015084053-A1 |
priorityDate | 2007-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 63.