http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20090092614-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44f04d319aaa6e66f240244bc905f452 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-325 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-3312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-334 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-33306 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-33324 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-325 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-00 |
filingDate | 2008-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_694f09643e6050722369393f8c5570b9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3416aeadcd841f73f77f51128b85eb18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22206fb63a14984be87c01b8d8e43fe7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0b01a035dcb344e63dab78ca05707869 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26613938230fba06960c5fa52b6fa631 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7143c0fd166e74327f0f7770b90a98a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_66732d1887573df7969b6e809c57be0d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5225ff7e9ca924082afa2d57db2a8e4f |
publicationDate | 2009-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20090092614-A |
titleOfInvention | Brush polyether-based polymers, preparation methods thereof and chemical sensors comprising the polymers |
abstract | The present invention provides a functional brush polymer compound represented by Chemical Formula 1, a method for preparing the same, and a chemical sensor device using the same. The functional brush polymer compound according to the present invention does not leach out of the active ingredient and the lipophilic functional group when used as a chemical sensor, and can be processed into various forms due to its excellent melting and solubility even without the addition of a plasticizer. It can be usefully used for chemical sensor elements, such as ion selective electrode, optical sensor, and gas sensor, for the purpose of detecting and analyzing it.n n n (I)n n n Wherein R 1 , R 2 , R 3 , R 4 , R 5 and R 6 are independently hydrogen, an alkyl group having 1 to 20 carbon atoms;n n n a and b are the content of the polyether unit (mol%), 0 <a ≦ 100, 0 ≦ b <100, and a + b = 100;n n n Y is H, an alkyl group having 1 to 20 carbon atoms, -ZPh (Q, T) or ego;n n n Q is trifluoroacetyl;n n n T is H, -R * OH, -R * CHO, -R * COOH, -R * COOR, -R * NHCOR or -R * CONHR, where R * is hydrogen, an alkyl group of 1 to 50 carbohydrates;n n n X is F, Cl, Br or I;n n n Z, W is -CH 2 SROCO-, -CH 2 SRCOO-, -CH 2 SRO-, -CH 2 SRNHCO-, -CH 2 SROCO (CH 2 ) 2 OCO-, -CH 2 SRCO-, -CH 2 SO 2 ROCO-, -CH 2 SO 2 RCOO-, -CH 2 SO 2 RO-, -CH 2 SO 2 RNHCO-, -CH 2 SO 2 ROCO (CH 2 ) 2 OCO-, -CH 2 SO 2 RCO-, -OCOROCO-, -OCORCOO-, -OCORO-, -OCORNHCO-, -OCOROCO (CH 2 ) 2 OCO-, -OCORCO-, -COOROCO-, -COORCOO-, -COORO-, -COORNHCO-, -COOROCO (CH 2 ) 2 OCO-, -COORCO-, -OROCO-, -ORCOO-, -ORO-, -ORNHCO-, -OROCO (CH 2 ) 2 OCO-, -ORCO-, -NHROCO-, -NHRCOO-, -NHRO -, -NHRNHCO-, -NHROCO (CH 2 ) 2 OCO-, -NHRCO-, -CH 2 ROCO-, -CH 2 RCOO-, -CH 2 RO-, -CH 2 RNHCO-, -CH 2 ROCO (CH 2 ) 2 OCO-, -CH 2 RCO-, -OC 6 H 4 ROCO-, -OC 6 H 4 RCOO-, -OC 6 H4 R O-, -OC 6 H 4 RNHCO-, -OC 6 H 4 ROCO (CH 2 ) 2 OCO-, -OC 6 H 4 RCO-, -OC 6 H 4 COOROCO-, -OC 6 H 4 COORCOO-, -OC 6 H 4 COORO-, -OC 6 H 4 COORNHCO-, -OC 6 H 4 COOROCO (CH 2 ) 2 OCO-, -OC 6 H 4 COORCO- or -OC 6 H 4 CONHROCO-, -OC 6 H 4 CONHRCOO-, -OC 6 H 4 CONHRO-, -OC 6 H 4 CONHRNHCO - made of a, -OC 6 H 4 CONHROCO (CH 2) 2 OCO-, -OC 6 H 4 CONHRCO- An aliphatic or aromatic derivative is selected from the group, wherein R is selected from the group consisting of hydrogen, alkyl groups of 1 to 20 carbon hydrogen. The weight average molecular weight of the chemical sensor functional brush polymer compound is 5,000 to 5,000,000, preferably 5,000 to 500,000. |