abstract |
The present invention, 27.6 parts by weight-36.2 parts by weight of polysilicate, 10.6 parts by weight or less of any one selected from epoxy and vinyl resin, 21.2 parts by weight-42.6 parts by weight of colloidal silica, -OH, -NH 2 , 10.6 parts by weight or less of an additive comprising at least one selected from the first group consisting of -COOH and at least one selected from the second group consisting of -C n F 2n + 1 and -SiR 3 Provides an anti-fingerprint coating for a stainless steel outer case of an appliance with improved anti-fingerprint and scratch resistance. |