abstract |
The present invention is to produce a shoe midsole with a silane-grafted resin to induce water cross-linking and spontaneous secondary crosslinking after molding, physical properties inevitably occur according to the elapsed time after molding of the foam, in particular permanent compression shrinkage The present invention relates to a method for producing a silane-grafted polyolefin resin and a shoe midsole foam using the same, wherein the deterioration of the silane-grafted polyolefin resin can be effectively controlled. Characteristics, in particular, the degradation of the permanent compression reduction characteristics has the advantage that it is greatly improved. |