http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20080104292-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee1c19da359446fb5c4f0458a57b783d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31667 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-3154 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0757 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-02118 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0755 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-027 |
filingDate | 2007-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7246ad63bf973f01fd98c9854a6228ab |
publicationDate | 2008-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20080104292-A |
titleOfInvention | Treating substrate having a hydrophilic region and a water-repellent region and a method for producing the same |
abstract | Provided is a treated substrate having on its surface a hydrophilic region and a water repellent region with high contrast. Also provided is a method for producing a treated substrate in a short period of time with a low amount of light without necessitating irradiation of a special device, high energy light or long time light.n n n (A) containing a compound (a) having at least one (meth) acryloyl group and a water-repellent moiety and a photopolymerization initiator is cured by using a treatment substrate having a hydrophilic region and a water repellent region on the surface of the substrate And a water repellent film having a film thickness of 0.1 to 100 nm. (A) is formed by forming a film containing the composition (A) on its surface by using a hydrophilic substrate or by making the surface hydrophilic by subjecting the surface of the substrate to hydrophilization and irradiating a part of the surface of the film with light, Curing the composition to form a water repellent film having a film thickness of 0.1 to 100 nm and removing the uncured composition (A) present on the surface of the substrate to expose a hydrophilic surface. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9391211-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9123818-B2 |
priorityDate | 2006-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.