Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-624 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 |
filingDate |
2007-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_145b04c4f011bd84bc19f151ff88e2ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e042836909918c7c397c20d36261ac9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_766e166b2eb95f1bd6dcffa74b142e29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fb2c2fe1620dc6b60042f6833c6866e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc8165743038b69134de3c85c124cae3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3d98e285fbf257f59363f76c277b263 |
publicationDate |
2008-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20080099888-A |
titleOfInvention |
Electrode Material for Secondary Battery and Manufacturing Method Thereof |
abstract |
The present invention provides an electrode material for a secondary battery having a structure in which sub-microsized electrode active material particles are evenly dispersed and bonded to the surface of the conductive material particles of several tens of micro-sizes.n n n The electrode material according to the present invention can provide sufficient electron migration path at the bonding site of the conductive material particles and the electrode active material and can improve the reversibility, thereby improving the charge and discharge efficiency, output characteristics and lifespan characteristics. In addition, various problems that may occur due to the aggregation and sedimentation of the electrode active material particles due to the lowering of dispersibility, such as a decrease in adhesion between the electrode mixture and the current collector, an increase in internal resistance, and a decrease in charge and discharge capacity, may be solved. You can. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210002756-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210122879-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190139339-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20130064288-A |
priorityDate |
2007-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |