Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c72d118f5664072de841f9c5c34b9d99 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2371-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2425-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F6-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-07 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 |
filingDate |
2006-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0de5b8db9eed10a85a65dad3681644e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_669e8ab4edebd0f26c7693c9fbdd2e84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_266e5de94cf405a51b739eefef8bf253 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49af4bd810951f5a645d86d010e1c13f |
publicationDate |
2008-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20080068018-A |
titleOfInvention |
A method for reducing the styrene content of a poly (arylene ether) / polystyrene blend, and an article comprising the thermoplastic resin obtained thereby |
abstract |
The poly (arylene ether) / polystyrene blend can be prepared by melt kneading the carboxylic acid compound, poly (arylene ether), and polystyrene to form a homogeneous blend, and steam stripping the homogeneous blend, The melt kneading is here carried out with a specific energy consumption of about 0.1 to about 0.3 kilowatt-hours per kilogram of blend. The method allows for the formation of a homogeneous blend while minimizing the styrene monomer content of the final blend. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010082998-A3 |
priorityDate |
2005-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |