Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_927c3131644244d81f82743c2a670aab |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12979 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12618 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12722 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12972 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C28-322 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C28-345 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C28-321 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D9-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C28-00 |
filingDate |
2006-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c008d7a40718682f3fb8dba403a7e4b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_465f293464afa813131ba0d61ead34fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bebcb9c7bcb7814020e6875d64ad7993 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1cf48872ad15bd639634d1816c85e62d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb87f51740e75cf95b9ccbf6c6b43698 |
publicationDate |
2008-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20080046742-A |
titleOfInvention |
Tin plated steel sheet and its manufacturing method |
abstract |
The tin-plated steel sheet has a plating layer containing tin on at least one surface of the steel sheet, and has a chemical conversion coating containing P and tin on the plating layer, and the deposition amount of the chemical conversion coating is 1.0 to 50 mg in terms of P per surface. / M 2 or more, the atomic ratio Sn / P of Sn and P obtained from the intensity of the P2p peak and the Sn3d peak of the chemical conversion coating film measured from the surface by X-ray photoelectron spectroscopy is 1.0 to 1.5, and the intensity of the P2p peak and the O1s peak The atomic ratio O / P of O and P calculated | required from is 4.0-9.0. The phosphoric acid chemical conversion treatment film of this tin-plated steel sheet can suppress the performance deterioration resulting from the growth of the tin oxide film of a surface layer instead of the conventional chromate coating film. |