Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b5aed51274edaa615a3f38619a3c6edf |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2323-42 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D71-34 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D71-34 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B31D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D67-00 |
filingDate |
2006-07-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53f0577c13a23133549e732aa1939a80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7fc3a876c6398413d00ac2d6222c77ed |
publicationDate |
2008-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20080034964-A |
titleOfInvention |
Manufacturing method of porous track membrane |
abstract |
Exposing the polymer film to the impact of heavy ions to provide a film having a track density, and etching the pores in the tracked film produced with the etching solution to maintain a turbulent flow, thereby obtaining a pore density corresponding to the track density. By providing a film having, a porous track membrane is produced. Alkali etching solutions are used that contain alkali metal salts at a concentration sufficient to raise the boiling point of the resulting alkali metal containing solution to a temperature in the range of about 100 to about 150 ° C. |