http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20070059609-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1bc8d5b80410c3a0594da023cfabcbe0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2331-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-088 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 2005-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_054292cfe2c950f97c4e9ef702597fd8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9609e66c21b67c2fe242ec3d6fea1571 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_839e9ccca724cf7a9ed2459b78d742b1 |
publicationDate | 2007-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20070059609-A |
titleOfInvention | Method for preparing high strength polyethylene-2,6-naphthalate fiber with improved leveling agent |
abstract | The present invention relates to a method for producing polyethylene naphthalate fibers having high strength and improved leveling agent by applying a high speed low temperature airjet to undrawn yarn. The process according to the invention comprises (A) spinning 20 to 200 solid phase polymerised polyethylene-2,6-naphthalate chips containing at least 85 mol% of ethylene-2,6-naphthalate units and having an intrinsic viscosity ranging from 0.80 to 1.20. Melting spinning at a draft ratio to produce a melt-emitting yarn; (B) solidifying the molten yarn through a delayed cooling zone and a rapid cooling zone to which a high speed low-temperature air jet is applied; (C) winding the yarn at a spinning speed such that the birefringence rate of the undrawn yarn is 0.001 to 0.015; And (D) multi-stretching the wound yarn to a total draw ratio of 4.0 or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180085408-A |
priorityDate | 2005-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.