http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20070027772-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0089 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F136-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-126 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F12-08 |
filingDate | 2005-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7431987c377f76974ca0fdde4dc4bc7d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31aa43efacbbcf8b7440452001fd6a99 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ed9e15194579074c60ee2cba908f590 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61df5f6fcac9c8358caa0175dfaa4d38 |
publicationDate | 2007-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20070027772-A |
titleOfInvention | Manufacturing method of impact reinforcing agent for flame retardant styrene resin having excellent appearance characteristics |
abstract | The present invention relates to a method for preparing an impact modifier of a flame retardant styrene resin having excellent injection appearance characteristics. A) preparing a butadiene-based rubber polymer having an average particle diameter of 1000 to 3000 GPa, a gel content of 70 to 90%, and a swelling index of 12 to 40 step; And b) 40 to 70 parts by weight of the butadiene rubber polymer, and 0.1 to 1.0 parts by weight of a graft crosslinking agent and 30 to 60 parts by weight of a styrene monomer at 40 to 60 ° C. for 2 to 5 hours in a row, reacting, and graft copolymerization. It relates to a method for producing a styrene-containing graft copolymer of the core shell type consisting of.n n n When the graft copolymer prepared by the production method of the present invention is used as an impact modifier of a flame retardant styrene resin, it is possible to provide a flame retardant styrene resin that is excellent in impact resistance and can be molded without appearance defects under various molding conditions. . |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101020087-B1 |
priorityDate | 2005-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links