http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20060132004-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f9a0a4a9748f1b5f0df8d23aeb1e2491 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B21-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F7-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-362 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F7-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-362 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B21-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F7-04 |
filingDate | 2005-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a82d0d245102a6ae1a64769b948a7264 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_221e30bd863932d08660eb7182844abc |
publicationDate | 2006-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20060132004-A |
titleOfInvention | Noncorrosive aids for aluminum soldering |
abstract | FIELD OF THE INVENTION The present invention relates to noncorrosive auxiliaries for the manufacture of aluminum and for the improvement of aluminum alloys based on alkali metal alumina fluorides, their preparation and their use.n n n According to the invention, the noncorrosive adjuvants contain a metal acid salt. To form the metal salts, metal compounds or transition elements of the main Group 2 to 5 elements of the periodic table are used as reactants in the form of their salts or oxides. For example, halides, nitrates, carbonates, sulfates, phosphates, borates, hexafluorosilicates or oxides are used. According to the invention, the metal compound is introduced into the reaction mixture of hydrofluoric acid and / or hydrated alumina and / or alkali metal compound. The time point at which the metal compound is added may vary depending on the degree of surface functionality desired. |