Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_132721b781afede2175d04e894580568 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-86 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-025 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 |
filingDate |
2006-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a975bba0a37068c469c1663adf8e5ff2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61e74b3d5cc80aa694a6ca2becce5229 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d5bf909317cd642c1c3f35ec7397898 |
publicationDate |
2006-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20060111384-A |
titleOfInvention |
Coextruded Laminated Foam and Its Molded Products |
abstract |
It is an object of the present invention to provide a coextruded laminated foam having a sufficient antistatic effect with high durability and excellent mechanical properties such as impact resistance and rigidity, buffering property and thermoforming.n n n The coextruded laminated foam has a polyolefin resin layer containing an antistatic agent on at least one side of a polystyrene resin foam layer having an apparent density of 100 g / L to 450 g / L and a continuous bubble ratio of 40% or less, and the polystyrene resin foam The polystyrene-based resin composition constituting the layer contains a styrene-based elastomer, the rubber component content in the polystyrene-based resin composition is 9 to 30% by weight, washing the ethanol aqueous solution of the polyolefin-based resin layer laminated surface of the coextruded laminated foam The surface resistivity after this is 1 × 10 13 Ω or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009145586-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009145586-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101142748-B1 |
priorityDate |
2005-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |