abstract |
The thermoplastic resin composition (Y) is (A) 20 to 64.9% by weight of an ethylene-based copolymer containing an ethylene-α-olefin copolymer, (B) 35 to 70% by weight of a metal hydroxide, and (C) a graft-modified ethylene-based polymer It contains 0.1-30 weight%, the resin composition which is excellent in a flame retardant effect, has good flexibility and flexibility, and is excellent in tensile property is obtained, and is suitable for an insulator and a sheath of an electric wire. In addition, the polymer composition (Z) is composed of 50 to 250 parts by weight of a metal hydroxide (BB), 0.1 to 40 parts by weight of a triazine compound (E), and a polyhydric alcohol (F) based on 100 parts by weight of a polymer (AA) such as a thermoplastic polymer or a thermosetting polymer. ) 0.1 to 40 parts by weight, and a polymer composition having a high flame retardant effect and a molded article thereof can be provided, which is suitable for insulators and sheaths of electric wires. |