http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050115199-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b32d5cce9fd3d4cf537cb8950eba1c5 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B24D18-0009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B24D7-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D7-00 |
filingDate | 2004-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aed3fa9421693e9633f86a763541be53 |
publicationDate | 2005-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050115199-A |
titleOfInvention | Grinding wheel having a pad |
abstract | The present invention relates to a grinding wheel for a grinding machine, and more particularly, to a grinding wheel having a pad as a substitute for reinforcing plates by applying a foamed resin to the back of the grinding wheel and pressing.n n n To this end, according to the present invention, in a grinding wheel in which abrasive pieces (2) are repeatedly stacked around a circular hub (30): a foamed resin (50) is applied to the rear surface (10a) of the grinding wheel (10) and then molded In the mold 60, the pressure is applied by the press 70 to form the pad 150. In the molding mold 60, the foaming conditions are between 90 ° C at room temperature and the foaming time is 3 seconds to 5 Minutes, the pressure applied is preferably from 0.5 to 7 kgf / cm 3, and the pad 150 is preferably dressing on a shelf to impart rotational stability. |
priorityDate | 2004-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |