http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050089462-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a49c208f818df616c962eed700d0305c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F7-56 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-26 |
filingDate | 2004-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_981bf1ae82d5b5a33f1cdfd4b9a615c6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd8a993ffcf07a75a16febb79a938eab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65f2617e750aff4f278610e6f64bc8e4 |
publicationDate | 2005-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050089462-A |
titleOfInvention | Manufacturing method for poly aluminium chloride silicate |
abstract | The present invention relates to a method for producing polyaluminum silicate using aluminum hydroxide, hydrochloric acid and silicate as a raw material, wherein the mixture obtained by adding aluminum hydroxide to a reactor containing hydrochloric acid and an aqueous silicate solution having a SiO 2 concentration of 10.0 wt% or less is 150-170. The present invention relates to a method for producing aluminum polysilicate chloride by heating at a temperature.n n n The method of the present invention has the effect of producing a high concentration of polyaluminum silicate silica in one simple step. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180115780-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101700412-B1 |
priorityDate | 2004-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.