http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050087995-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b7d93678875a7a0cf6a82fa1fb3dabb5 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2204-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C11-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-076 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-076 |
filingDate | 2004-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5814c28bf15492d09b4a80e992e97a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09cf78222005325a0aaebc0ace0aa265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0466687288072399a0db759f70dc4b5f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d5358aaf101495a4e767e969c7e9eec1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_62ae30a92864ef725318f8f4cc467fd6 |
publicationDate | 2005-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050087995-A |
titleOfInvention | Process for manufacturing abrasive |
abstract | The present invention relates to a method for producing an exfoliating abrasive for producing an exfoliating abrasive used to remove exfoliation generated in various parts of the human body such as the sole of the foot.n n n The present invention is foamed selected from carbonates or sulfates based on 60 to 95% by weight of waste glass powder, 1 to 48% by weight of sericite, and 100 parts by weight of basic material made by mixing 1 to 40% by weight of ocher or kaolinite. An additive mixing step of mixing 0.3 to 33 parts by weight of an additive consisting of a preparation, boron oxide and sodium silicate; Pulverizing the mixture to 150 mesh or less; Kneading step of kneading by adding a binder selected from CMC, PVA, water glass to the pulverized mixture; A molding step of molding the kneaded mixture; Firing the molded body at 400 to 750 ° C. and then foaming at 800 to 1050 ° C .; Subsequently, the annealing step to stabilize the foam at 500 ~ 700 ℃ and then unwind at 20 to 40 ℃; Etc., the exfoliating abrasive prepared according to the manufacturing method can function as antibacterial, far-infrared radiation, cleaning, etc., and also does not lose the exfoliation function until all worn out. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160052306-A |
priorityDate | 2004-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 198.