http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050074523-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8c8f42c3e4c81674b2d70588e80a2af9
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-026
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-527
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-522
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-062
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-52
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04
filingDate 2003-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9cbb356c708e7c85b0f378b76ae0777
publicationDate 2005-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20050074523-A
titleOfInvention Process for producing blended cements with reduced carbon dioxide emissions
abstract As a method of producing the compounding cement,n n n Portland cement is fully mixed with fine supplement cement-based materials and microfillers selected from blast furnace slag, fly ash, quartz, silica, amorphous silicon dioxide, limestone and recycled concrete materials and possibly moisture reducing agents for the dry cement mixture Contains cement,n n n And in the first step, the supplement material is ground to a dry surface on a specific surface of at least 1000 cm 2 / g (Blaine), and in the second step, the supplemented material ground is dried with a highly reactive cement mixture of at least 20% by weight of the total grinding weight. Grinding in the state characterized in that to obtain a specific surface of more than 3000 cm 2 / g (Blaine),n n n The highly reactive cement mixture contains cement and at least one of the polymer and Si0 2 -containing microfiller components in the form of a powdery water-reducing agent, the mixture having already been treated in the grinder with a vibrating grinding medium and the cement And wherein the particles are subjected to a number of influence stimuli to provide cement particles with increased surface energy and chemical reactivity.
priorityDate 2002-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457698762
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID280
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID2695409
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID2695409
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635

Total number of triples: 30.