http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050039977-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_51f78002fa61363c73515efdf2af05fa |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2031-736 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2403-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2509-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2043-5816 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2061-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B13-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B7-88 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-52 |
filingDate | 2003-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2624487b4e17fe3715a9883c6f6064d1 |
publicationDate | 2005-05-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050039977-A |
titleOfInvention | Method of producing an abrasive |
abstract | A method for producing an abrasive used for grinding such as a yellow bar plating body is disclosed. The abrasive production method comprises the steps of crushing the oasis sieving sieve; Blending 350 to 420 g of the filtered oasis with 260 to 380 g of resin and 280 to 380 g of silicon carbide, and mixing in a mixer for 10 to 40 minutes; The mixture is mixed is put into a hydraulic pressure and compressed to a pressure of 1,500 ~ 2,000kg / ㎠; Firstly heating the compacted mixture in an electric mold at a temperature of 120 to 140 ° C. for 30 to 60 minutes; Second heating for 30 to 60 minutes at a temperature of 150 to 180 ° C. in the same electric mold after the first heating; Tertiary heating for 30 to 60 minutes at a temperature of 80 to 100 ° C. in the same electric mold after secondary heating; And cutting both ends by moving the hardened abrasive to the lathe. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101341069-B1 |
priorityDate | 2003-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.