http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050034919-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F12-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F12-08 |
filingDate | 2003-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2cb16584feec3a5166b4acdd952e28b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac046e91d2dbf70edbe2e2aad8ad1c57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c8ec6cac31e9036c94218109615bbe4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_42ca5eff913dfd2b147a55ad3c40dd64 |
publicationDate | 2005-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050034919-A |
titleOfInvention | Rubber modified styrene resin having high strength and gloss and preparing method thereof |
abstract | The present invention relates to a rubber-modified styrene-based resin having a bimodal particle size distribution and a method for producing the same, wherein the butadiene rubber polymer and a styrene-based monomer are dissolved in an organic solvent. A pre-graft polymerization step of graft polymerization of a predetermined amount of the mixed solution using a polymerization initiator; And a graft polymerization step of graft polymerization by further adding the remaining amount of the mixed solution to the pre-graft polymer. Made of a rubber-modified styrene resin according to the present invention has an excellent impact strength and gloss. |
priorityDate | 2003-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |