http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050031196-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fb4c3f4767460093b3aa6d7251b5a5ac |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00482 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-26 |
filingDate | 2003-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_912bda8b3daba073a758ff23b7662798 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a65a91fef82d15241f46305e3f18cc2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7f4e3890ff02a6028fb2ba0de05e4d1f |
publicationDate | 2005-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050031196-A |
titleOfInvention | Incombustible composition, incombustible material for architecture using the same and preparing method thereof |
abstract | The present invention relates to a non-combustible composition, a non-combustible molded article for construction using the same and a method for manufacturing the same, more specifically, 1 to 80% by weight of organic or inorganic fibers, 1 to 80% by weight of fly ash or bottom ash, and 1 to 1 flame retardant. Non-combustible composition comprising 80% by weight and 1 to 60% by weight of a flame-retardant curing agent, the method of producing a non-combustible molded article that is mixed with the non-combustible composition, and then molded by a roller press or an autoclave and the non-combustible prepared by the method It relates to a molded article.n n n According to the present invention, it is environmentally friendly while using waste materials, and it is excellent in hardness, strength, water resistance, etc. by reinforcing the disadvantages physically and chemically compared to the existing materials, and is inexpensive, and above all, non-combustible performance according to the composition ratio Excellent incombustible compositions and building finishes and interior materials prepared therefrom can be provided. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020218631-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102040361-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102040361-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110627520-A |
priorityDate | 2003-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.