http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050025748-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e5ad8562c578b061df7a2c3aee9d0e24 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-14 |
filingDate | 2003-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45e82c0f713b7c035f6dc5c9842dc0a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3df4faf02fd1829b609e56f48d861d3e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea0db7ffd3f75967d3d0048dd3c4d80e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_705ea31653e9c346e61a908315e29843 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3ce80aeb5ab7a3ec516845b243c05ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5799b705b6e58e3c3cdb2da6cdce3ea4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d978eb718d33e5a9722126d761f41d13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d20fb4b413b5aa0f3ca6bd03c4c77595 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e99b2b7f6ce7b7c8371e8d1caf34958c |
publicationDate | 2005-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20050025748-A |
titleOfInvention | Hydrothermal-electrochemical synthesis method of licoo2 using saccharin |
abstract | The present invention relates to a hydrothermal electrochemical synthesis method of LiCoO 2 used not only as an active material of a lithium secondary battery, but also as a stabilizing material that suppresses the dissolution of cathodes in a molten carbonate fuel cell, and more particularly, in hydrothermal electrochemical synthesis, Saccharin-based LiCoO by adding saccharin to aqueous solution lowers the synthesis temperature by increasing crystallinity and adhesion, eliminating the use of autoclave, and shortening the synthesis time by applying a pulse current instead of direct current. It relates to a hydrothermal electrochemical synthesis method of 2 .n n n Sequence electrochemical method for the synthesis of LiCoO 2 with saccharin according to the present invention is a method for synthesis of LiCoO 2 using the sequence electrochemical synthesis method, the addition of saccharin, lithium salt and a cobalt salt, or an aqueous solution obtained by dissolving a cobalt powder in water Characterized in that.n n n In the hydrothermal electrochemical synthesis method of LiCoO 2 using saccharin according to the present invention, a pulse current is applied during hydrothermal electrochemical synthesis. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200114361-A |
priorityDate | 2003-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 51.