http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20040105047-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aafe0172ffd94d3486c518b0709bb2b3 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-53 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 |
filingDate | 2003-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2384170386a1acb12c757f25812c33b8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf283fb6f3d7c7527c2fe6c3ef452aba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a78a545b21244e535d3817b32b775f0 |
publicationDate | 2004-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20040105047-A |
titleOfInvention | The Method of Manufacturing ABS Resin Having Improved Whiteness and Thermal Stability |
abstract | ABS resin composition excellent in whiteness and thermal stability according to the present invention is introduced into the conjugated diene-based monomers by introducing ion-exchanged water and an emulsifier in which a polymerization initiator, an electrolyte and a molecular weight regulator are dissolved, the average particle diameter is 2500 ~ 4000 kPa, gel A large-diameter conjugated diene rubber latex having a content of 60 to 90 wt% and a swelling index of 10 to 40 was prepared, and 25 to 70 parts by weight of an aromatic vinyl compound and a vinyl cyanide compound were added to 30 to 75 parts by weight of the rubber latex by a step administration method. G-ABS was prepared by graft emulsion polymerization by continuous injection, and coagulated by adding 0.05-1 parts by weight of a radical initiator to the g-ABS, followed by dehydration and drying to prepare a powder form, and g of the powder form. Injecting the SAN and the additive to the ABS together-kneading at a temperature of 190 ℃ to 230 ℃. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180077438-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100755441-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101469268-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100963086-B1 |
priorityDate | 2003-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.