http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20040012119-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_455dbca6b5c773163243bc3be116d48c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_42bd7dccf9bdf2d2d1c326f1d92165d7 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-28 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-0048 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-24 |
filingDate | 2002-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b70615890c39e1d0f49f216c2aabab1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_88d28272bc96da5b48c7aca0746e0ba1 |
publicationDate | 2004-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20040012119-A |
titleOfInvention | Method for manufacturing of fire retardant interior material by using waste paper and cotton |
abstract | The present invention is a waste paper, waste fiber is put into the water dissociated into the flame retardant is added to a certain ratio of the clay powder, ganban stone powder, coal ash fine powder was mixed and stirred by a molding method, such as papermaking method to a certain thickness in the form of paper or plate The method relates to a method for manufacturing a flame retardant interior material, characterized in that it is manufactured by dehydration, drying by blowing with a blower, and then subjected to a surface treatment process, specifically, waste paper or waste fiber 75-85% by weight as a raw material. And dissociate it until it reaches a certain level, add a known size filler filler fragrance, and add 4-8% by weight of sodium hydrogen carbonate (NaHCO 3 ) as a flame retardant, and add ocher powder as a functional additive. 4-8% by weight, 4-6% by weight of ganbanite powder and 3-5% by weight of coal ash are stirred and then molded into paper or 2-5 mm thick plates and dehydrated. It is manufactured by surface treatment by drying by sending air to the blower at below 40 ℃. In case of fire, the flame retardant effect is excellent due to the separation reaction of sodium hydrogen carbonate and the interaction of loess, elvan, and coal ash used as functional additives. In general, antibacterial, deodorant, and anti-gom farm can be used for health benefits, and the soundproofing, heat insulation, and humidity control functions are superior to other interior materials, resulting in a pleasant interior effect. New flame retardant interior materials with high cost and low cost. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100868992-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011010905-A1 |
priorityDate | 2002-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.