http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030085168-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3e99c243f3278902e3628ac188005ade |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2501-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2503-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-02 |
filingDate | 2002-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f028e82f81f52863782a1cafeb10b0f |
publicationDate | 2003-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20030085168-A |
titleOfInvention | The process of manufacturing paper, cotton, mineral mixed healthy bioceramic padding |
abstract | The present invention is a recycled cotton formed by cutting natural cotton or chemical cotton or discarded cotton fibers or chemical fibers waste to a predetermined length, and is a raw material of paper mulberry pulp paper material of high viscosity and strong binding to recycled cotton formed on a cotton batter (紙 料 液) Mixed with and mixed with loamy, jade and biotite powders as far-infrared emitters, and prepared by papermaking with a paper machine. It has a heat insulation effect, water absorption effect, excellent binding force of raw materials, excellent durability, heat resistance and washing resistance, and the manufacturing method of health cotton containing fine material and soft far-infrared radiation substance.n n n The present invention is 15% (weight ratio) of fine pulverized jade powder 15% (weight ratio), biotite powder 15 to 15% (weight ratio) of paper pulp mixed with wood pulp mixed with 2: 1 20% (weight ratio) of fiber wool is mixed with the mixed stock of% (weight ratio) and 35% (weight ratio) of yellow clay powder in the state of coarse precipitate precipitated in the underground storage for 24 to 48 hours. 10% (by weight) rosin of the material was added and coagulated and precipitated for 5 hours to produce cotton balls in a paper machine in a conventional manner, and dried paper was laminated up and down to a thickness of 2-3 mm to form a Fuji, then 10 cm wide. It is cut to the size of the batter with a cotton wool to manufacture a health cotton with a combination of Hanji, fiber material cotton, functional minerals. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006137662-A1 |
priorityDate | 2002-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 184.