http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030059983-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d7762fa08acbcf2a7cc64762e559dc90 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-10 |
filingDate | 2002-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_268c9ebefbd659932d7bae0a24cd87fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e15a72a599cc0dab7189547b28d4d44 |
publicationDate | 2003-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20030059983-A |
titleOfInvention | A acrylic resin composition and the method of manufacturing thereof |
abstract | The present invention is produced by mixing the acrylic resin of MMA, BMA, IBMA, EDMA in a predetermined weight ratio so that the acrylic resin composition is easily dissolved in the plasticizer, it is possible to produce not only hard acrylic resin but also soft acrylic resin. It is to improve the effectiveness of the acrylic resin product.n n n At least one or more compounding combinations of the acrylic resins in a weight ratio of MMA > BMA > IBMA > EDMA, and then mixed with a solvent in a weight ratio of 20 to 100 ml acrylic resin composition to be dissolved in a plasticizer After mixing the acrylic resin of MMA, BMA, IBMA, EDMA blended in a predetermined weight ratio in the weight ratio of the solvent 20 to 100ml, the temperature is maintained at 100 ~ 200 ℃ 1 ~ while heating and stirring Reacting for about 3 hours to produce chips through an extrusion process; It is intended to implement a method for producing an acrylic resin composition, characterized in that consisting of; a second step of processing the acrylic resin into a powder by cutting and grinding the chip while maintaining the temperature below -0 ℃. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190122060-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100655322-B1 |
priorityDate | 2002-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 34.