http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030035728-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1bc8d5b80410c3a0594da023cfabcbe0
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D07B2501-2046
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S57-902
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2505-022
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-693
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-48
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F8-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-088
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02J1-22
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-28
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-02
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-14
filingDate 2001-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a43785891ef13953ddae739bf61c3d60
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b1096a76a795f19891754a57f1acb5e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_00b2038b1a112ef6bcaac185a6aca450
publicationDate 2003-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20030035728-A
titleOfInvention Process for production of a polyester multifilament yarn for the industrial use
abstract The present invention relates to a method for producing industrial polyester multifilament yarn, and melt-extruded polyester chip having an intrinsic viscosity of 0.90 to 1.2 through a spinneret to pass a suitable heating section below the spinneret, followed by radial in-out cooling (Radial). It is a method of producing high strength, low shrinkage polyester yarn of 1,000 denier or more under high speed spinning speed of 2,000m / min by applying solidified cooling just before winding and solidifying by cooling gas by In to Out Quenching) method. .n n n The stretched polyester multifilament yarn produced according to the method of the present invention has a fineness uniformity with a filament cross section diameter variation coefficient of 4.0% or less.n n n In addition, the high modulus low shrinkage polyester industrial yarn of the present invention exhibits high strength and low shrinkage, and the treatment cord formed therefrom has excellent shape stability and strength, and thus is useful as a reinforcement material for rubber products including tires. Can be used.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100627960-B1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20050064612-A
priorityDate 2001-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID15066111
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID55477
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID411275696
http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID55477

Total number of triples: 28.