http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030032696-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aafe0172ffd94d3486c518b0709bb2b3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F292-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F292-00 |
filingDate | 2001-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_56a874025fe1537a34294b5874dd819a |
publicationDate | 2003-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20030032696-A |
titleOfInvention | Method of Preparing Rubber Modified Polystyrene Resin Composition With High Gloss and Impact Resistance |
abstract | The method for preparing a rubber-modified polystyrene resin composition of the present invention comprises a raw material solution consisting of 80 to 95% by weight of styrene monomer (A) and 5 to 20% by weight of butadiene rubber polymer (B) and an organically treated clay mineral (C). A first step of converting the rubber component phase into dispersed particles by polymerizing at a temperature of 90-150 ° C. in a first reactor; And a second step of adding the polymer of the first reactor to a second reactor maintained at 130-180 ° C. to complete the polymerization. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20040042353-A |
priorityDate | 2001-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 73.