http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030018719-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7a75913df71baf69d68e952f02bc7762 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_833774e493efdb57fc2735eb6fc76acc http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5f99151cc6ccca54bc1f2967ad582c43 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-844 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-04 |
filingDate | 2001-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_afb74f2f5d1c2e0264ead0437aa7d457 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2494735c5158779bcf753528350d78a9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cfbea47b91749e1dd85e47715ff17b02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f912e7643a560b6695ddb771cdc5ebf |
publicationDate | 2003-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20030018719-A |
titleOfInvention | Method for manufacturing organic light emitting device encapsulated by polyxylene film |
abstract | The present invention relates to a method of manufacturing an organic light emitting device having excellent stability and extended lifespan by encapsulating an organic light emitting device using a polyxylene thin film having high thermal stability and resistance to gas permeability.n n n Method for manufacturing an encapsulated organic light emitting device using a polyxylene thin film according to the present invention comprises the steps of vacuum depositing an organic layer constituting a hole transport layer, a light emitting layer and an electron transport layer on an ITO-coated anode in turn, for the cathode on the organic layer Depositing a metal electrode and at least one of a poly-para-xylene layer or a poly-para-xylene derivative layer on the cathode is deposited and polymerized in a vacuum at 25 ° C. or lower; It is characterized by encapsulating by forming a.n n n According to the present invention, the poly-para-xylene thin film or a derivative thin film thereof may be used to manufacture a stable organic light emitting device that is completely blocked from moisture, oxygen, and small particles. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180052797-A |
priorityDate | 2001-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 33.