http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20020085414-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_609fd9072a780eefd8a9c077fd1541c6 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06N2211-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06N3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S428-904 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06N3-0059 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06N7-04 |
filingDate | 2001-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b83d801cca7c6abfabf723485ee3a82 |
publicationDate | 2002-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20020085414-A |
titleOfInvention | Fragnance Slow-Releasing Artificial Leather and Preparing Method Thereof |
abstract | The present invention relates to a Westward synthetic leather and a method for manufacturing the same, and more particularly, to a Westward artificial leather and a method for producing the fragrance release agent contained in the color printing layer and / or surface coating layer. ,n n n In the artificial leather composed of a resin sheet having a color / pattern printed layer and a surface coating layer, the sustained-oriented artificial leather according to the present invention comprises 0.1 to 25% by weight of the printed layer based on the weight of the printed layer described above. And / or 0.1 to 40% by weight of the fragrance is contained in the surface coating layer based on the weight of the coating layer.n n n The manufacturing method is an artificial leather manufacturing method comprising a resin substrate providing step, a foaming step, a printing step, and a surface treatment step, wherein the aromatic release agent is 0.1 to 10% by weight in the printing step and / or the surface treatment step, respectively. Consisting of incorporation,n n n Since the surface coating layer itself functions as a millipore film that controls the directional characteristics, and the fragrance is emitted only by friction or pressure on the surface of the artificial leather, it can exhibit good directionality with use over a long period of time, There is little unpleasant unique solvent odor, so that it can effectively meet the taste of consumers. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102357750-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100797031-B1 |
priorityDate | 2001-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 177.