http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20020077146-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ac17835c97e6c72213815ca74845386 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-443 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D13-06 |
filingDate | 2002-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4859cd9150a49581617d87b27dac2e00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86155b8ddf87fa2ea740e00ab6f4ec47 |
publicationDate | 2002-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20020077146-A |
titleOfInvention | Electrodeposition coating process |
abstract | The present invention provides a relatively low coating film (deposited film) formed on the surface of a substrate by partially forming an electrodeposition film on the surface of the substrate to be coated using a modified lead-free cationic electrodeposition coating composition. A first electrodeposition step to have a transition temperature; A second electrodeposition step of forming an electrodeposition film on the uncoated portion of the substrate surface using the modified lead-free cationic electrodeposition coating composition such that the deposited film has a relatively high glass transition temperature; And it relates to an electrodeposition coating method comprising the step of baking the electrodeposition coating (curing). The electrodeposition coating process reduces the film thickness difference between the inner surface and the outer surface, improves the smoothness of the outer surface even when a small amount of the coating composition is used, and has a low volatile organic substance content (VOC) and a metal ion content for the environment. There is little impact. |