Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0373 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-00 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 |
filingDate |
2002-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb3a08004e14f1bd7d02035cdd71195e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2223f9bef3501807fc369c19a877bf5 |
publicationDate |
2002-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20020077110-A |
titleOfInvention |
Liquid crystal polyester resin composition |
abstract |
At a shear rate of 1000 sec −1 and a flow temperature of + 40 ° C., obtained by blending 10 to 100 parts by weight of inorganic filler in fiber form and 10 to 100 parts by weight of inorganic filler in plate form per 100 parts by weight of liquid crystal polyester resin. A liquid crystal polyester resin composition having an apparent melt viscosity of 10 to 100 Pa.sec, wherein the liquid crystal polyester resin contains 30 mol% or more of the repeating structural unit of formula (A 1) and has a flow temperature of 270 ° C. to 400 ° C., and forms a fiber Of the inorganic filler has an average fiber diameter of 0.1 to 10 μm and a number average fiber length of 1 to 100 μm, the plate-shaped inorganic filler has an average particle size of 5 to 20 μm, and the amount of the inorganic filler in the fiber form (F ) Liquid crystal polyester whose ratio (F / P) of the compounding amount (P) of the inorganic filler in the form of a plate satisfies the equation: 0 < F / P < 0.5 or 1.6 < Terpolymer composition:n n n [Formula A1] |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120112089-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9109111-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210055782-A |
priorityDate |
2001-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |