Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2314-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-142 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate |
2002-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee6b803dcd31edca5da108f0d0270319 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54c33e2c1c51dc5c3dc99aa0728148e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba6d33d09f15f27055ecc63546c46854 |
publicationDate |
2002-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20020070111-A |
titleOfInvention |
Polypropylene resin composition and process for producing the same |
abstract |
Propylene-based substrate having an intrinsic viscosity [η] of 2.0 to 5 dl / g measured at 135 ° C. tetralin and a melting point (Tm) defined from the peak temperature of the melting curve measured with a differential scanning calorimeter. 20 to 98 parts by weight of the polymer (A) and an intrinsic viscosity [η] measured in tetralin at 135 ° C. are 0.80 to 1.8 dl / g, and a melting point defined from the peak temperature of the melting curve measured by a differential scanning calorimeter ( A polypropylene resin composition containing 2 to 80 parts by weight of a propylene-based polymer (B) having a Tm) of 160 to 166 ° C, and a melt flow rate of 0.5 to 20 g / 10 minutes, and a method for producing the same. |