http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20020049872-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c4b5184b7a8fe02a0c2cc4e509230214 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09F2003-0272 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09F3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G09F3-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F3-00 |
filingDate | 2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9611767e1674602212dc8cac131a026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73caa8cff827a047042335e86d09be07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53d9d3db31f5bcedee291dbc5e635cc6 |
publicationDate | 2002-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20020049872-A |
titleOfInvention | Label and recycling method of plastic bottle to which the label is attached |
abstract | The present invention relates to a label and a method for regenerating a plastic bottle equipped with the label, wherein the ink layer can be removed from an alkaline hot water having a pH of 9.0 or higher and a temperature of 50 to 100 ° C. on either side of the thermoplastic resin film. It provides a label characterized in that it comprises a.n n n The label according to the present invention can easily remove the ink layer by depositing an ink layer containing a soluble or swellable compound in an alkaline hot water in an alkaline hot water, and also after using the PET bottle equipped with the label. Since the ink layer on the label can be easily removed, the PET bottle and the label from which the ink has been removed can be easily melt-extruded to be made into regenerated thermoplastic polymer pellets, and the recycled pellet prepared by the above method does not contain ink. Because it is not in the state, it can be used without any deterioration in physical properties for regeneration molding. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10800898-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10800897-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11548996-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11008434-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11008435-B2 |
priorityDate | 2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links