Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dd7c27b9ec61781656e6f039702fd568 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fba3bbed3ee9a59359b2189e7a0b81a3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2369-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-307 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-46 |
filingDate |
2000-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54181236b1bf489e5ddbefa7836cefe6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7cc6d602b0c4b5e5c90079554c5c663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe3c7bf237703cc17468eb4749495ffa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_08f428a9e6363e25411321c8364dcab1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f56b6f17ad70fc01799973b78786389 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a578339b0057cb646d56c82afa0e42d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_27d1ec5a4badde655b86f7f3a2bc5489 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f09ef97fff1f5d3775b1581aedb8db8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93f37512fd344b190ac0e3289678904b |
publicationDate |
2002-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20020007012-A |
titleOfInvention |
Process for the preparation of polycarbonate by microwave |
abstract |
The present invention relates to a method for producing a polycarbonate resin using microwave, and more particularly, in a method for producing a polycarbonate resin in which solid phase polymerization is carried out by crystallizing a prepolymer polymerized from an aromatic dihydroxy compound and a diaryl carbonate. Preparing a prepolymer having a specific range of viscosity average molecular weight; Crystallizing the prepolymer into crystalline particles to have a specific range of crystallinity; The present invention relates to a method for producing a high molecular weight polycarbonate resin having excellent quality in a short time by solid phase polymerization while applying microwaves having a frequency of 900 MHz to 2.45 GHz to the prepolymer crystalline particles. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100561743-B1 |
priorityDate |
2000-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |