http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-200192827-Y1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c306624d33bba81b1425da7a359a1568 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2075-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61N2005-066 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B68G7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A47C3-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B68G7-00 |
filingDate | 2000-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2000-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ab04b260f271a99726867152be7e7c9 |
publicationDate | 2000-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-200192827-Y1 |
titleOfInvention | To ore coating manage sponge to use a chair |
abstract | The present invention relates to a method for manufacturing a chair using a sponge formed by coating a natural jade and finely ground ore powder, in particular a crushing step of obtaining a far-infrared radiator powder raw material, and a mixture obtained by mixing the powder raw material and the adhesive resin The jadeite processing step obtained by the process step, the crushed stone and then melted by cooling it in the setting frame and processing, and a plurality of jadeite receiving grooves are arranged to have a polyurethane foam and arranged while maintaining a predetermined interval on the setting surface Cushion material forming process step of forming the selected shape and shape by injection molding uniformly apply the far-infrared radiation adhesive resin to the entire outer surface or a specific selected site and then dried for a predetermined time to form a cushioning material having a far-infrared radiation layer; , Which consists of a plurality of exterior members injection molded into a set shape After assembling each other to the frame and seating and fixing the cushioning material obtained through the cushioning material forming step on the upper and inner surfaces of the seat plate and the back plate joined by a plurality of fastening elements, respectively, the outer surface is covered with a seat cover material of the set material. It is characterized by consisting of the final assembly process step of forming a cover assembly.n n n According to the present invention described above, there is no wear or damage of the far-infrared radiation layer due to friction and inadvertent use due to frequent contact when the user is seated, and the desired amount of far-infrared radiation can be obtained. It stimulates metabolism by magnetic force along with far-infrared rays, and facilitates blood circulation, and quickly discharges various wastes and heavy metals remaining in the body to sweat and urine, and promotes growth and stimulates menstrual blood. (氣) The reinforcement effect, there is an effect that can be achieved by reducing fatigue due to stress relief. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015050370-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015050370-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100808236-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20000072652-A |
priorityDate | 2000-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links