Predicate |
Object |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-26 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-26 |
filingDate |
2001-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2001-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20010111018-A |
titleOfInvention |
Polybutadiene and process for producing the same |
abstract |
The raw polybutadiene having a Tcp / ML 1 + 4 ratio (Tcp: 5% toluene solution viscosity at 25 ° C, ML 1 + 4 ; Mooney viscosity at 100 ° C) of 2.5 or more was denatured in the presence of a transition metal catalyst, , A modified polybutadiene having a high-sheath and low-trans structure at the 2- content and improved properties such as cold flow properties. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7863385-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7884155-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7700691-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20040070058-A |
priorityDate |
2000-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |