http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20010100278-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e20306987b7e2fce0d5aabbfe12ea20e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-06 |
filingDate | 2000-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d00efc80362bdc7cec414b90ed6835f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a6745ec94b26548fd9e78b2e0b611f8 |
publicationDate | 2001-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20010100278-A |
titleOfInvention | Tire cure bladder composition |
abstract | The present invention relates to a rubber composition for tire vulcanizing brader, comprising 100 parts by weight of isobutylene bromide-p-methylstyrene copolymer, iodine adsorption of 82 to 125 g / kg and dibutyl phthalate absorption of 78 to 125 ml / 100 g. 40 to 70 parts by weight of black, 5 to 15 parts by weight of castor oil, 10 to 40 parts by weight of master batch for isobutylene-p-methylstyrene copolymer containing fatty acid amide mixture, natural fatty acid calcium combined with amide ester wax It consists of 1 to 5 parts by weight of salt (Calcium salts of natural fatty acids in combination with amide ester waxes) and ordinary additives. It can prevent the physical property deviation of rubber caused by undispersed and the adhesiveness of rubber becomes high. To improve the fluidity to eliminate the poor workability of the adhesive by which it is possible to obtain an effect of improving the thermal aging resistance can be consequently prolong the service life of the tire probe ladder. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100650011-B1 |
priorityDate | 2000-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 33.