Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-00 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 |
filingDate |
1998-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2000-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20000075698-A |
titleOfInvention |
Hydrosilylation cross linking of thermoplastic elastomer |
abstract |
The present invention relates to a method for preparing a thermoplastic elastomer by hydrosilylation crosslinking of an elastic component, wherein the use of an elastomer containing this non-conjugated diene and having a Mooney viscosity in the range of 45 to 100 MST is a high level. To provide a combination of crosslinking and improved physical properties. These improvements are achieved even at low concentrations of hydrosilylation catalysts. |