http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20000062784-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-28 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-44 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-07 |
filingDate | 2000-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2000-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20000062784-A |
titleOfInvention | Silicone composition and silicone pressure sensitive adhesive |
abstract | The present invention relates to a polyorganosiloxane (A) containing from 20 to 55 parts by weight of an average of at least two silicon-bonded alkenyl groups per molecule, consisting essentially of an O 3 consisting of R 3 3 SiO 1/2 units and SiO 4/2 units 45 to 80 parts by weight of nopolysiloxane resin (B), wherein the total amount of components (A) and (B) is 100 parts by weight), an average of at least two silicon-bonded molecules per molecule, in an amount sufficient to cure the composition Organohydrogenpolysiloxane (C) having a hydrogen atom, silicon pressure sensitive comprising 25 to 200 parts by weight of silica filler (D) having an average surface area of less than 25 m 2 / g and a catalytic amount of hydrosilylation catalyst (E) Provided is a silicone composition for preparing an adhesive. Each R 3 is independently selected from monovalent hydrocarbons and monovalent halogenated hydrocarbon groups. The molar ratio of R 3 3 SiO 1/2 units to SiO 4/2 units in the organopolysiloxane resin is from 0.6: 1 to 1.5: 1 and the resin contains less than 2 mol% of alkenyl groups. The sum of the average number of silicon-bonded alkenyl groups per molecule in component (A) and the average number of silicon-bonded hydrogen atoms per molecule in component (C) is at least 4.0. The present invention provides a silicone pressure sensitive adhesive comprising the reaction product of the above described composition. The present invention includes components (A) to (E) in two or more parts, provided that component (A) and component (B) contain components (A) when the component (B) contains an alkenyl group. C) and component (E) are not present in the same part], a multi-part silicone composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180137501-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100853550-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100739001-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170067799-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101106522-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101067257-B1 |
priorityDate | 1999-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.