http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20000045850-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e0412713ae7ec4661e9923881f9502d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-542 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-67 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B1-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-18 |
filingDate | 1998-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57e81f1084d45db3fcf6598e195717c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7489cc37dce65154e4fad8d3119dac36 |
publicationDate | 2000-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20000045850-A |
titleOfInvention | Antimicrobial artificial stone composition and preparation method thereof |
abstract | The present invention relates to an antimicrobial artificial stone composition and a method for producing the same, wherein the composition of the present invention comprises the following composition.n n n end. 100 parts by weight of a thermosetting unsaturated polyester resin having a viscosity of 1 to 4 poise at room temperaturen n n I. Natural stone crushed 200 to 600 parts by weightn n n All. 300 to 700 parts by weight of inorganic fillern n n la. 0.1 to 2 parts by weight of inorganic antibacterial agentn n n hemp. 0.05 to 3 parts by weight of a high temperature curing catalyst and a cobalt acceleratorn n n bar. 0.1 to 3 parts by weight of silane coupling agentn n n four. 10 parts by weight or less of pigmentn n n In the preparation method of the present invention, the liquid component and the solid component of the composition are separately mixed for 10 to 20 minutes, the liquid raw material is poured on the solid component and mixed for 3 to 20 minutes, and the mixture is press-molded while applying vibration to heating. After curing, polishing the surface of the cured molding.n n n The antimicrobial artificial stone produced according to the present invention has a similar mechanical properties and appearance compared to the conventional natural stone and artificial stone, and the antibacterial activity is greatly improved. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8980149-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100422788-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100487628-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011090268-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20010044300-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018124427-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20100085881-A |
priorityDate | 1998-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.